Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 120 MPa @Strain 0.200 %, Temperature 600 °C |
17400 psi @Strain 0.200 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Yield | 120 MPa @Strain 1.00 %, Temperature 500 °C |
17400 psi @Strain 1.00 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | >= 120 MPa @Strain 0.200 %, Thickness 0.200 - 1.50 mm |
>= 17400 psi @Strain 0.200 %, Thickness 0.00787 - 0.0591 in |
|
Aleris 55HX® Aluminum (5005-H14) Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ.. |
|||
Tensile Strength, Yield | >= 120 MPa @Strain 0.200 %, Thickness 1.50 - 3.00 mm |
>= 17400 psi @Strain 0.200 %, Thickness 0.0591 - 0.118 in |
|
Aleris 55HX® Aluminum (5005-H14) Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ.. |
|||
Tensile Strength, Yield | >= 120 MPa @Strain 0.200 %, Thickness 3.00 - 5.00 mm |
>= 17400 psi @Strain 0.200 %, Thickness 0.118 - 0.197 in |
|
Aleris 55HX® Aluminum (5005-H14) Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ.. |