Tensile Strength, Yield 85.0 MPa

@Strain 0.200 %,
Temperature 500 °C
12300 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 85.0 MPa

@Strain 0.200 %,
Temperature 500 °C
12300 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 85.0 MPa

@Strain 0.200 %,
Temperature 500 °C
12300 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Tensile Strength, Yield 85.0 MPa

@Temperature 23.0 °C
12300 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66  (Unverified Data**)
Zytel® 103FHSA NC010 is a heat stabilized, lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 85.0 MPa

@Temperature 23.0 °C
12300 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66  (Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 85.0 MPa

@Temperature 23.0 °C
12300 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers