Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 136 MPa @Strain 0.200 %, Temperature 300 °C |
19700 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 136 MPa @Strain 0.200 %, Temperature 300 °C |
19700 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Tensile Strength, Yield | 136 MPa @Temperature 816 °C |
19700 psi @Temperature 1500 °F |
ASTM E8 |
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |