Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1378 MPa @Strain 0.200 % |
199900 psi @Strain 0.200 % |
700°F Temper Temperature |
Latrobe Lescalloy® 4335+V VAC-ARC High Strength Alloy Steel 4335+V VAC-ARC is a low alloy steel with good strength and high hardenability. In addition, uniform properties are obtained in large sections. The alloy can be heat treated to strength values with.. |