Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 952 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
Transverse, typical |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wi.. |
|||
Tensile Strength, Yield | 950 - 1050 MPa @Strain 0.2 % |
138000 - 152000 psi @Strain 0.2 % |
as built, Z direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Tensile Strength, Yield | 950 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
Double Age |
Crucible Compaction Metals P/M 625M Corrosion Resistant Alloy P/M 625M (chemically, UNS N07626) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The a.. |