Mechanical Properties Metric English Comments
Tensile Strength, Yield 149 MPa

@Strain 1.00 %,
Temperature 500 °C
21600 psi

@Strain 1.00 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 149 MPa

@Strain 1.00 %,
Temperature 500 °C
21600 psi

@Strain 1.00 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..