Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1030 MPa @Strain 0.200 % |
150000 psi @Strain 0.200 % |
40-42 HRC |
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica.. |
|||
Tensile Strength, Yield | 1030 MPa @Strain 0.200 % |
150000 psi @Strain 0.200 % |
H1075 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Tensile Strength, Yield | 1030 MPa @Strain 2.00 %, Temperature 316 °C |
150000 psi @Strain 2.00 %, Temperature 600 °F |
H900 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Tensile Strength, Yield | 1030 MPa @Strain 0.200 % |
150000 psi @Strain 0.200 % |
H1075 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Tensile Strength, Yield | 1030 MPa @Strain 2.00 %, Temperature 316 °C |
150000 psi @Strain 2.00 %, Temperature 600 °F |
H900 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Tensile Strength, Yield | 1030 MPa @Strain 0.200 % |
150000 psi @Strain 0.200 % |
H1075 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Tensile Strength, Yield | 1030 MPa @Strain 2.00 %, Temperature 316 °C |
150000 psi @Strain 2.00 %, Temperature 600 °F |
H900 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Tensile Strength, Yield | 1034 MPa @Strain 0.200 %, Thickness 9.50 mm |
150000 psi @Strain 0.200 %, Thickness 0.374 in |
Hardened at 1850°F for 30 min, oil quenched and tempered for 4 hrs at 1000°F [plate, transverse] |
AK Steel 410 Cb Martensitic Stainless steel AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra.. |