Polymer Property : Tensile Strength, Yield = 162 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 162 MPa

@Strain 1.00 %,
Temperature 400 °C
23500 psi

@Strain 1.00 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Tensile Strength, Yield 162 MPa

@Strain 0.200 %,
Temperature 100 °C
23500 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Tensile Strength, Yield 162 MPa

@Temperature 871 °C
23500 psi

@Temperature 1600 °F
Vacuum
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..