Tensile Strength, Yield 1650 MPa

@Strain 0.200 %
240000 psi

@Strain 0.200 %
50 HRC
EDRO #7 Shock Resistant S7 Tool Steel
EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s..