Polymer Property : Tensile Strength, Yield = 171000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1180 MPa

@Strain 0.200 %
171000 psi

@Strain 0.200 %
44 HRC
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel
Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity)..