Polymer Property : Tensile Strength, Yield = 1731 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1731 MPa

@Temperature 24.0 °C
251100 psi

@Temperature 75.2 °F
Dry
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape
Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel
Tensile Strength, Yield 1731 MPa

@Temperature 23.0 °C
251100 psi

@Temperature 73.4 °F
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..