Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1200 MPa @Temperature 204 °C |
174000 psi @Temperature 400 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |
|||
Tensile Strength, Yield | 1200 - 1400 MPa @Strain 0.2 % |
174000 - 203000 psi @Strain 0.2 % |
after modified H900 heat treatment, XY direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Tensile Strength, Yield | 1200 - 1400 MPa @Strain 0.2 % |
174000 - 203000 psi @Strain 0.2 % |
after modified H900 heat treatment, Z direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |