Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 185 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 185 MPa

@Strain 0.200 %,
Temperature 200 °C
26800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Tensile Strength, Yield 185 MPa

@Strain 0.200 %,
Temperature 200 °C
26800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4439 Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms.
Tensile Strength, Yield 185 MPa

@Strain 0.200 %,
Temperature 100 °C
26800 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Yield 185 MPa

@Strain 1.00 %,
Temperature 100 °C
26800 psi

@Strain 1.00 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 185 MPa

@Strain 1.00 %,
Temperature 100 °C
26800 psi

@Strain 1.00 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Tensile Strength, Yield 185 MPa

@Temperature 100 °C
26800 psi

@Temperature 212 °F
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in ..
Tensile Strength, Yield 185 MPa

@Strain 0.200 %,
Temperature 593 °C
26800 psi

@Strain 0.200 %,
Temperature 1100 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Tensile Strength, Yield 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
50 mm/min; ISO 527-1/-2
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Tensile Strength, Yield 185 MPa

@Strain 0.200 %,
Temperature 593 °C
26800 psi

@Strain 0.200 %,
Temperature 1100 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)