Polymer Property : Tensile Strength, Yield = 1860 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1860 MPa

@Strain 0.200 %
270000 psi

@Strain 0.200 %
hardness of 58 HRC
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel
Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are ..