Polymer Property : Tensile Strength, Yield = 18700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 129 MPa

@Strain 0.200 %,
Temperature 500 °C
18700 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Tensile Strength, Yield 129 MPa

@Strain 0.200 %,
Temperature 500 °C
18700 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Yield 129 MPa

@Temperature 260 °C
18700 psi

@Temperature 500 °F
ATI Wah Chang Zircadyne® Alloy Zr 702
Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A..