Mechanical Properties Metric English Comments
Tensile Strength, Yield 1312 MPa

@Strain 0.200 %,
Thickness 3.20 mm
190300 psi

@Strain 0.200 %,
Thickness 0.126 in
60% cold reduction
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..