Polymer Property : Tensile Strength, Yield = 1930 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1930 MPa

@Strain 0.200 %,
Temperature 482 °C
280000 psi

@Strain 0.200 %,
Temperature 900 °F
Solution Annealed Plus Aged, AC
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel
UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica..
Tensile Strength, Yield 1930 MPa

@Strain 0.200 %,
Time 10800 sec
280000 psi

@Strain 0.200 %,
Time 3.00 hour
Solution Annealed Plus Aged, AC
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel
UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica..