Polymer Property : Tensile Strength, Yield = 196 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 196 MPa

@Strain 1.00 %,
Temperature 200 °C
28400 psi

@Strain 1.00 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Yield 196 MPa

@Temperature 149 °C
28400 psi

@Temperature 300 °F
ATI Wah Chang Zircadyne® Alloy Zr 702
Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A..
Tensile Strength, Yield 196 MPa

@Temperature 260 °C
28400 psi

@Temperature 500 °F
ATI Wah Chang Zircadyne® Alloy Zr 705
Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other ..