Mechanical Properties Metric English Comments
Tensile Strength, Yield 1370 MPa

@Strain 0.200 %
198000 psi

@Strain 0.200 %
44-48 HRC
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel
Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica..