Polymer Property : Tensile Strength, Yield = 19900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 137 MPa

@Strain 0.200 %,
Temperature 200 °C
19900 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 137 MPa

@Strain 0.200 %,
Temperature 200 °C
19900 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 137 MPa

@Strain 0.200 %,
Temperature 200 °C
19900 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 137 MPa

@Temperature 982 °C,
Time 45700 sec
19900 psi

@Temperature 1800 °F,
Time 12.7 hour
As Welded, Solution Annealed, and Aged; Weld/Weld Fracture; 0.2% Offset
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Yield 137 MPa

@Strain 1.00 %,
Temperature 300 °C
19900 psi

@Strain 1.00 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..