Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.0 MPa

@Strain 50.0 %
2030 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PL471 45 Shore D, Injection Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 14.0 MPa

@Strain 5.00 %
2030 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® UM622 General Purpose Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 14.0 MPa

@Strain 5.00 %
2030 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® UM622 Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 14.0 MPa

@Strain 300 %
2030 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® S85A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue..
Tensile Strength, Yield 14.0 MPa

@Strain 100 %
2030 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® S95A Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tensile Strength, Yield 14.0 MPa

@Strain 50.0 %
2030 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PL471 Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..