Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Temperature 400 °C |
20300 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Temperature 600 °C |
20300 psi @Strain 0.200 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Temperature 100 °C |
20300 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Temperature 100 °C |
20300 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Thickness 20.0 - 100 mm |
20300 psi @Strain 0.200 %, Thickness 0.787 - 3.94 in |
Typical Strength |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Tensile Strength, Yield | 140 MPa @Temperature 80.0 °C |
20300 psi @Temperature 176 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |