Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2137 MPa @Temperature 71.0 °C |
309900 psi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, T5A120 Carbon Tape Hexcel designation: TXX120-12"-F515; Fiber: IM6Information provided by HexCel |