Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 2250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.5 MPa

@Strain 300 %
2250 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® M88A55 Polyester Type Polyurethane Elastomer
The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl..
Tensile Strength, Yield 15.5 MPa

@Strain 300 %
2250 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® M88A15 Polyester Type Polyurethane Elastomer
The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl..