Polymer Property : Tensile Strength, Yield = 2280 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.7 MPa

@Strain 100 %
2280 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 194A L series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 15.7 MPa

@Strain 50.0 %
2280 psi

@Strain 50.0 %
ASTM D638
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang.