Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.0 MPa @Strain 300 % |
3340 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 2090A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength, Yield | 23.0 MPa @Strain 300 % |
3340 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1090A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 23.0 MPa @Temperature 871 °C |
3340 psi @Temperature 1600 °F |
|
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 23.0 MPa @Strain 10.0 % |
3340 psi @Strain 10.0 % |
ASTM D638 |
Samyang Triel® 5650 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5650 is an extrusion grade.Information provided by Samyang. |