Mechanical Properties Metric English Comments
Tensile Strength, Yield 236 MPa

@Thickness 12.7 mm,
Temperature 427 °C
34200 psi

@Thickness 0.500 in,
Temperature 801 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Tensile Strength, Yield 236 MPa

@Strain 0.200 %,
Temperature 500 °C
34200 psi

@Strain 0.200 %,
Temperature 932 °F
Typical annealed sample; short time elevated temp.
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..