Polymer Property : Tensile Strength, Yield = 24.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.4 MPa

@Strain 1.00 %
3540 psi

@Strain 1.00 %
ASTM D95
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L
Tensile Strength, Yield 24.4 MPa

@Strain 300 %
3540 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® 695A15N Polyester Type Polyurethane Elastomer
This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes..
Tensile Strength, Yield 24.4 MPa

@Strain 300 %
3540 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® 695A15 Polyester Type Polyurethane Elastomer
This grade contains a hydrolytic stabilizer. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are ..