Mechanical Properties Metric English Comments
Tensile Strength, Yield 167 MPa

@Strain 1.00 %,
Temperature 300 °C
24200 psi

@Strain 1.00 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 167 MPa

@Strain 1.00 %,
Temperature 200 °C
24200 psi

@Strain 1.00 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 167 MPa

@Strain 0.200 %,
Temperature 200 °C
24200 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 167 MPa

@Strain 0.200 %,
Temperature 200 °C
24200 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Tensile Strength, Yield 167 MPa

@Strain 1.00 %,
Temperature 200 °C
24200 psi

@Strain 1.00 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 167 MPa

@Strain 1.00 %,
Temperature 300 °C
24200 psi

@Strain 1.00 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Tensile Strength, Yield 167 MPa

@Strain 0.200 %,
Temperature 200 °C
24200 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Yield >= 167 MPa

@Temperature 250 °C
>= 24200 psi

@Temperature 482 °F
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength, Yield 167 MPa

@Temperature 538 °C
24200 psi

@Temperature 1000 °F
ASTM E8
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..