Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 168 MPa @Strain 0.200 %, Temperature 371 °C |
24400 psi @Strain 0.200 %, Temperature 700 °F |
Plate |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |