Polymer Property : Tensile Strength, Yield = 25100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 173 MPa

@Temperature 538 °C
25100 psi

@Temperature 1000 °F
ATI Allegheny Ludlum AL 453™ Stainless Steel
Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum
Tensile Strength, Yield 173 MPa

@Temperature 371 °C
25100 psi

@Temperature 700 °F
ATI Wah Chang Zircadyne® Alloy Zr 705
Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other ..