Tensile Strength, Yield 180.00 MPa

@Strain 0.200 %
26107 psi

@Strain 0.200 %
as cast
Wieland Portagold Casting Alloy
Gold casting alloyApplications: inlays/onlays, crownsDental
Tensile Strength, Yield 180.00 MPa

@Strain 0.200 %
26107 psi

@Strain 0.200 %
hardened
Wieland Portagold Casting Alloy
Gold casting alloyApplications: inlays/onlays, crownsDental