Polymer Property : Tensile Strength, Yield = 269 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 269 MPa

@Thickness 12.7 mm,
Temperature 760 °C
39000 psi

@Thickness 0.500 in,
Temperature 1400 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 269 MPa

@Strain 0.200 %,
Thickness 6.35 - 12.7 mm
39000 psi

@Strain 0.200 %,
Thickness 0.250 - 0.499 in
Aleris Alustar H131 Aluminum Alloy
Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts.
Tensile Strength, Yield 269 MPa

@Strain 0.200 %,
Thickness 12.7 - 50.8 mm
39000 psi

@Strain 0.200 %,
Thickness 0.500 - 2.00 in
Aleris Alustar H131 Aluminum Alloy
Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts.
Tensile Strength, Yield 269 MPa

@Strain 0.200 %,
Thickness 50.83 - 76.2 mm
39000 psi

@Strain 0.200 %,
Thickness 2.001 - 3.00 in
Aleris Alustar H131 Aluminum Alloy
Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts.
Tensile Strength, Yield 269 MPa

@Strain 0.200 %,
Thickness 6.35 - 12.7 mm
39000 psi

@Strain 0.200 %,
Thickness 0.250 - 0.499 in
Aleris Alustar H136 Aluminum Alloy
Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts. H136 has a higher elongation than H131 and so provides better protec..
Tensile Strength, Yield 269 MPa

@Strain 0.200 %,
Thickness 12.7 - 50.8 mm
39000 psi

@Strain 0.200 %,
Thickness 0.500 - 2.00 in
Aleris Alustar H136 Aluminum Alloy
Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts. H136 has a higher elongation than H131 and so provides better protec..
Tensile Strength, Yield 269 MPa

@Strain 0.200 %,
Thickness 50.83 - 76.2 mm
39000 psi

@Strain 0.200 %,
Thickness 2.001 - 3.00 in
Aleris Alustar H136 Aluminum Alloy
Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts. H136 has a higher elongation than H131 and so provides better protec..
Tensile Strength, Yield 269 MPa

@Thickness 6.35 mm,
Temperature 538 °C
39000 psi

@Thickness 0.250 in,
Temperature 1000 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Tensile Strength, Yield 269 MPa

@Thickness 12.7 mm,
Temperature 760 °C
39000 psi

@Thickness 0.500 in,
Temperature 1400 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..