Polymer Property : Tensile Strength, Yield = 29.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa

@Temperature 23.0 °C
4210 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..
Tensile Strength, Yield 29.0 MPa

@Strain 300 %
4200 psi

@Strain 300 %
ASTM D412
Teknor Apex Laripur® LPR 5260EG Thermoplastic Polyurethane
Features: - Excellent performance under extreme and aggressive environments - Superior abrasion and cut resistance - Resistance to chemical, microbial attack and hydrolysis - Excellent flexibility a..
Tensile Strength, Yield 29.0 MPa

@Temperature 23.0 °C
4210 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612  (Unverified Data**)
Zytel® LC6210 BK010 is a highly toughened, heat stabilized polyamide 612 for extrusion, blow molding or processing by other techniques requiring high melt viscosity. It was previously coded Zytel®..