Mechanical Properties Metric English Comments
Tensile Strength, Yield 296 MPa

@Thickness 1.57 mm
43000 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP511 Glass Fabric
Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat..
Tensile Strength, Yield 296 MPa

@Strain 0.200 %,
Temperature 500 °C
42900 psi

@Strain 0.200 %,
Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 296 MPa

@Temperature 538 °C
43000 psi

@Temperature 1000 °F
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability ..
Tensile Strength, Yield 296 MPa

@Temperature 316 °C
43000 psi

@Temperature 600 °F
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability ..
Tensile Strength, Yield 296 MPa

@Temperature 1112 °C
43000 psi

@Temperature 2034 °F
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel
Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica..
Tensile Strength, Yield 296 - 386 MPa

@Strain 0.200 %,
Thickness 1.02 - 2.92 mm
42900 - 56000 psi

@Strain 0.200 %,
Thickness 0.0400 - 0.115 in
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily..
Tensile Strength, Yield 296 MPa

@Temperature 23.0 °C
43000 psi

@Temperature 73.4 °F
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..