Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 213.1 MPa @Temperature 538 °C |
30910 psi @Temperature 1000 °F |
Autogenously Welded plate, 1.6mm thick |
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |