Polymer Property : Tensile Strength, Yield = 318 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 318 MPa

@Temperature 200 °C
>= 46100 psi

@Temperature 392 °F
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Tensile Strength, Yield 318 MPa

@Thickness 12.7 mm,
Temperature 25.0 °C
46100 psi

@Thickness 0.500 in,
Temperature 77.0 °F
0.2% Offset
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..