Mechanical Properties Metric English Comments
Tensile Strength, Yield 319 MPa

@Temperature 93.0 °C
46300 psi

@Temperature 199 °F
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F155; Fiber: 450-1/2Information provided by HexCel
Tensile Strength, Yield 319 MPa

@Strain 0.200 %,
Temperature 93.0 °C
46300 psi

@Strain 0.200 %,
Temperature 199 °F
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Tensile Strength, Yield 319 MPa

@Thickness 25.4 mm,
Temperature 25.0 °C
46300 psi

@Thickness 1.00 in,
Temperature 77.0 °F
0.2% Offset
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..