Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 221 MPa @Thickness 9.50 mm, Temperature 538 °C |
32100 psi @Thickness 0.374 in, Temperature 1000 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |