Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2310 MPa @Strain 0.200 % |
335000 psi @Strain 0.200 % |
hardened to 60 RC |
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for.. |