Polymer Property : Tensile Strength, Yield = 362 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 362 MPa

@Temperature 150 °C
>= 52500 psi

@Temperature 302 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all..
Tensile Strength, Yield >= 362 MPa

@Temperature 150 °C
>= 52500 psi

@Temperature 302 °F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6
Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Tensile Strength, Yield 362 MPa

@Thickness 19.1 mm,
Temperature 25.0 °C
52500 psi

@Thickness 0.752 in,
Temperature 77.0 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..