Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 252 MPa

@Temperature 150 °C
>= 36500 psi

@Temperature 302 °F
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F
Information provided by PEAK Werkstoff GmbH
Tensile Strength, Yield 252 MPa

@Thickness 25.4 mm,
Temperature 371 °C
36500 psi

@Thickness 1.00 in,
Temperature 700 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..