Tensile Strength, Yield 375 MPa

@Strain 0.200 %
54400 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4742 High Temperature Ferritic Stainless Steel
Good scaling resistance and can be subjected to reducing sulphur environments without risk. Subject to 475°C embrittlement and grain coarsening at temperatures above 950°C. s-phase may form afte..