Mechanical Properties Metric English Comments
Tensile Strength, Yield 392 MPa

@Treatment Temp. 427 °C,
Time 3.60e+6 sec
56900 psi

@Treatment Temp. 801 °F,
Time 1000 hour
0.2%. Room temp test after thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 392 MPa

@Temperature -54.0 °C
56900 psi

@Temperature -65.2 °F
Dry
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel