Tensile Strength, Yield >= 396 MPa

@Temperature 20.0 °C
>= 57400 psi

@Temperature 68.0 °F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6
Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Tensile Strength, Yield 396 MPa

@Thickness 12.7 mm,
Temperature 316 °C
57400 psi

@Thickness 0.500 in,
Temperature 601 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield 396 MPa

@Strain 0.200 %,
Temperature 900 °C
57400 psi

@Strain 0.200 %,
Temperature 1650 °F
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Yield 396 MPa

@Treatment Temp. 427 °C,
Time 1.44e+7 sec
57400 psi

@Treatment Temp. 801 °F,
Time 4000 hour
0.2%. Room temp test after thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..