Mechanical Properties Metric English Comments
Tensile Strength, Yield 273 MPa

@Thickness 25.4 mm,
Temperature 260 °C
39600 psi

@Thickness 1.00 in,
Temperature 500 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..