Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.50 MPa

@Strain 50.0 %
653 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 3085AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tensile Strength, Yield 4.50 MPa

@Strain 50.0 %
653 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 3085A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..