Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 40.00 MPa @Temperature 22.2 °C |
5802 psi @Temperature 72.0 °F |
Cured Neat Resin Property, 1 hour @ 70°C/158°F, Conditioning: Dry; ISO R527 |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |