Polymer Property : Tensile Strength, Yield = 41.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa

@Temperature 23.0 °C
5950 psi

@Temperature 73.4 °F
50%RH; ASTM D638
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6  (Unverified Data**)
Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers