Mechanical Properties Metric English Comments
Tensile Strength, Yield 410.00 MPa

@Strain 0.200 %
59465 psi

@Strain 0.200 %
hardened
Wieland Porta PressOver PFM Alloy
High gold alloy for veneering with IMAGINE® h.e. press ceramicApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, acrylic veneeringDental